TPE THERMOLAST® K TC4FRN KRAIBURG TPE GERMANY
12
Technical Data Sheet
| flammability | Test Condition | Test Method | Test Result |
|---|---|---|---|
| UL flame retardant rating | 3.0mm | UL 94 | V-0 |
| elastomer | Test Condition | Test Method | Test Result |
|---|---|---|---|
| tensile strength | Yield | ISO 37 | 2.00 Mpa |
| elongation | Break | ISO 37 | 550 % |
| Permanent compression deformation | 100°C,24hr | ISO 815 | 84 % |
| 70°C,24hr | ISO 815 | 29 % | |
| 23°C,72hr | ISO 815 | 9.0 % | |
| tear strength | ISO 34-1 | 13 kN/m |
| hardness | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Shore hardness | ShoreA | ISO 7619 | 36 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.