Polyester, TS Glasrod HIR

0

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
densityASTMD7921.90 g/cm³
Water absorption rateASTMD5700.10 %
Impact resistanceTest ConditionTest MethodTest Result
Impact strength of cantilever beam gapASTMD2563200 J/m
Mechanical propertiesTest ConditionTest MethodTest Result
Tensile modulusASTMD6382.07E+06 MPa
tensile strengthYieldASTMD638621 MPa
Flexural modulusASTMD79027600 MPa
bending strengthYieldASTMD790689 MPa
shear strengthASTMD73224.1 MPa
Electrical performanceTest ConditionTest MethodTest Result
dielectric strengthASTMD1493.1 kV/mm
dielectric constantASTMD1505.00
arc resistanceASTMD495150 sec
Thermal performanceTest ConditionTest MethodTest Result
ASTMD6966E-06 cm/cm/°C
thermal conductivityASTMC1770.29 W/m/K
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.