Technical Data Sheet
Uncured Properties | Test Condition | Test Method | Test Result |
---|
GelTime | | | 36 min |
density | | | 1.08 g/cm³ |
Viscosity | | | 0.55 Pa·s |
physical property | Test Condition | Test Method | Test Result |
---|
StyreneContent | | | 44 % |
hardness | Test Condition | Test Method | Test Result |
---|
Barcol Hardness | | ASTM D2583 | 39 |
Supplementary Information | Test Condition | Test Method | Test Result |
---|
GeltoPeak | | | 6.0 min |
PeakExotherm | | | 185 °C |
THIXOTROPIC INDEX | | | 2.50 |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
Tensile modulus | | ASTM D638 | 3380 MPa |
tensile strength | | ASTM D638 | 85.5 MPa |
elongation | Break | ASTM D638 | 4.0 % |
Flexural modulus | | ASTM D790 | 3930 MPa |
bending strength | | ASTM D790 | 141 MPa |
Impact resistance | Test Condition | Test Method | Test Result |
---|
Impact strength of cantilever beam gap | | ASTM D4812 | 220 J/m |
Thermal performance | Test Condition | Test Method | Test Result |
---|
Heat distortion temperature | | ASTM D648 | 91.7 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.