plas
Log In

ASA PRL ASA-GP1 Polymer Resources Ltd.

0

Technical Data Sheet

impact performanceTest ConditionTest MethodTest Result
Impact strength of cantilever beam gap23°C,3.18mmASTM D256190 J/m
mechanical propertiesTest ConditionTest MethodTest Result
tensile strengthYield,3.18mmASTM D63846.9 MPa
elongationYield,3.18mmASTM D6386.0 %
elongationBreak,3.18mmASTM D63825 %
Bending modulus3.18mmASTM D7902210 MPa
bending strength3.18mmASTM D79075.8 MPa
thermal performanceTest ConditionTest MethodTest Result
Hot deformation temperature0.45MPa,Unannealed,6.40mmASTM D64896.1 °C
Hot deformation temperature1.8MPa,Unannealed,6.40mmASTM D64887.8 °C
Physical propertiesTest ConditionTest MethodTest Result
melt mass-flow rate220°C/10.0kgASTM D12385.0to15 g/10min
Shrinkage rateMD:3.18mmASTM D9550.40to0.70 %
densityASTM D7921.07 g/cm³
hardnessTest ConditionTest MethodTest Result
Rockwell hardnessR-ScaleASTM D785103
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.