Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|
density | | ASTMD792 | 1.42 g/cm³ |
density | | ASTMD792 | 1.42 g/cm³ |
hardness | Test Condition | Test Method | Test Result |
---|
Shore Hardness | Shore A | ASTMD2240 | 82 |
Shore Hardness | Shore A | ASTMD2240 | 82 |
flammability | Test Condition | Test Method | Test Result |
---|
Limiting Oxygen Index | | ASTMD2863 | 30 % |
Limiting Oxygen Index | | ASTMD2863 | 30 % |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
tensile strength | | ASTMD638 | 19.0 MPa |
elongation | Break | ASTMD638 | 330 % |
tensile strength | | ASTMD638 | 19.0 MPa |
elongation | Break | ASTMD638 | 330 % |
aging | Test Condition | Test Method | Test Result |
---|
Changes in tensile stress during fracture in air | | IEC60811 | -12 % |
Change rate of tensile strength | | ENI018100 | 12 % |
Changes in tensile stress during fracture | | ENI018100 | -15 % |
Change rate of tensile strength in air | | IEC60811 | 13 % |
Changes in tensile stress during fracture in air | | IEC60811 | -12 % |
Change rate of tensile strength | | ENI018100 | 12 % |
Changes in tensile stress during fracture | | ENI018100 | -15 % |
Change rate of tensile strength in air | | IEC60811 | 13 % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.