Technical Data Sheet
物理性能 | Test Condition | Test Method | Test Result |
---|
AcrylonitrileContent-Bound | | 内部方法 | 33.0 % |
Stabilizer | | | Non-staining |
可溶性-inMEK | | | 100 % |
密度 | | | 0.980 g/cm³ |
门尼粘度 | ML1+4,100°C | ASTMD1646 | 62 MU |
弹性体 | Test Condition | Test Method | Test Result |
---|
拉伸应力 | 300%应变7 | ASTMD412 | 11.4 MPa |
抗张强度 | 屈服2 | ASTMD412 | 27.3 MPa |
抗张强度 | 屈服3 | ASTMD412 | 27.0 MPa |
抗张强度 | 屈服4 | ASTMD412 | 27.8 MPa |
伸长率 | 断裂5 | ASTMD412 | 620 % |
伸长率 | 断裂6 | ASTMD412 | 580 % |
伸长率 | 断裂7 | ASTMD412 | 560 % |
撕裂强度 | | ASTMD624 | 56.9 kN/m |
压缩永久变形 | 100°C,70hr | ASTMD395 | 55 % |
拉伸应力 | 300%应变5 | ASTMD412 | 9.32 MPa |
拉伸应力 | 300%应变6 | ASTMD412 | 10.5 MPa |
老化 | Test Condition | Test Method | Test Result |
---|
空气中拉伸强度的变化率 | 100°C,70hr | ASTMD865 | -14 % |
空气中极限伸长率的变化率 | 100°C,70hr | ASTMD865 | -38 % |
空气中硬度计硬度的变化率 | 邵氏A,100°C,70hr | ASTMD865 | 4.0 |
拉伸强度的变化率 | 100°C,70hr,在ASTM#1油中 | ASTMD471 | -11 % |
拉伸强度的变化率 | 100°C,70hr,在ASTM#3油中 | ASTMD471 | -28 % |
极限伸长率的变化率 | 100°C,70hr,在ASTM#1油中 | ASTMD471 | -28 % |
极限伸长率的变化率 | 100°C,70hr,在ASTM#3油中 | ASTMD471 | -28 % |
硬度计硬度的变化率 | 支撐A,100°C,70hr,在ASTM#1油中 | ASTMD471 | 1.0 |
硬度计硬度的变化率 | 支撐A,100°C,70hr,在ASTM#3油中 | ASTMD471 | -9.0 |
体积变化 | 100°C,70hr,ASTM标准油(1号) | ASTMD471 | 0.40 % |
体积变化 | 100°C,70hr,ASTM标准油(3号) | ASTMD471 | 16 % |
硬度 | Test Condition | Test Method | Test Result |
---|
肖氏硬度 | 邵氏A2 | ASTMD2240 | 71 |
肖氏硬度 | 邵氏A3 | ASTMD2240 | 72 |
肖氏硬度 | 邵氏A4 | ASTMD2240 | 73 |
热性能 | Test Condition | Test Method | Test Result |
---|
热损耗 | | ASTMD5688 | 0.20 % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.