LDPE ExxonMobil™  100AC EXXONMOBIL SAUDI

56
  • Properties:
    optical performance
  • Usages:
    film
    chip
    Vegetable and fruit packaging bags
    T-shirt packaging bag
    Display packaging
    Light shrink film
    General applications

Technical Data Sheet

optical performance Test ConditionTest MethodTest Result
Haze ratioASTM D-10035.5 %
glossASTM D-245710 %
Basic performanceTest ConditionTest MethodTest Result
density埃克森美孚方法0.9225 g/cm³
melt mass-flow rateASTM D-12382.0 g/10min
Mechanical propertiesTest ConditionTest MethodTest Result
elongation at breakASTM D-882350 %
elongation at breakASTM D-882580 %
Secant modulusASTM D-882220 Mpa
Secant modulusASTM D-882250 Mpa
Dart impactASTM D-1709A75 g
Elmendorf tear strengthASTM D-1922180 g
Elmendorf tear strengthASTM D-1922120 g
tensile strength ASTM D-88227 Mpa
tensile strength ASTM D-88222 Mpa
Thermal performanceTest ConditionTest MethodTest Result
melting temperature埃克森美孚方法109 °C
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.