Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|
density | | ASTM D792 | 1.20 g/cm³ |
density | | ISO 2781 | 1.20 g/cm³ |
water content | | 内部方法 | <0.10 % |
melt mass-flow rate | | ISO 1133 | 15to40 g/10min |
hardness | Test Condition | Test Method | Test Result |
---|
Shore hardness | Shore A | ASTMD2240 | 78 |
Shore hardness | | ISO 868 | 78 |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
tensile strength | | ISO 527-2 | 24.0 MPa |
tensile strength | | ISO 527-2 | 4.00 MPa |
tensile strength | | ISO 527-2 | 5.00 MPa |
Tensile strain | Break | ISO 527-2 | 650 % |
Wear amount | | ISO 4649 | 25.0 mm³ |
elastomer | Test Condition | Test Method | Test Result |
---|
elongation | Break | ASTMD412 | 750 % |
tear strength | | ASTM D624 | 70.0 kN/m |
tear strength | | ISO 34-1 | 70 kN/m |
tensile strength | | ASTMD412 | 4.00 MPa |
tensile strength | | ASTMD412 | 5.50 MPa |
tensile strength | Yield | ASTMD412 | 20.0 MPa |
Thermal performance | Test Condition | Test Method | Test Result |
---|
Glass Transition Temperature | | ISO 11357-2 | -32.0 °C |
melting temperature | | 内部方法 | 125to135 °C |
melting temperature | | 内部方法 | 130to140 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.