PC NH-3200 FW9661 Samsung Cheil South Korea
101
Form:Granules
Properties:
Glass fiber reinforcedFlame retardant
Typical Applications:
Audio and video equipmentLaptopElectronic and Electrical Applications
Product Description
Certificates(0)
Datasheet
Product Description
| Typical Applications: | Audio and video equipment | Laptop | Electronic and Electrical Applications |
| Properties: | Glass fiber reinforced | Flame retardant |
Certificates
No Data...
Technical Data Sheet
| flammability | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| UL flame retardant rating | 0.75 mm | UL 94 | V-0 | |
| 0.830mm | UL 94 | V-0 | ||
| 3.0 mm | UL 94 | V-0 | ||
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| bending strength | --5 | ISO 178 | 150 | Mpa |
| --4 | ASTM D790 | 150 | Mpa | |
| Bending modulus | --5 | ISO 178 | 6000 | Mpa |
| --4 | ASTM D790 | 5900 | Mpa | |
| elongation | Break | ISO 527-2/5 | 3.0 | % |
| Break3 | ASTM D638 | 3.0 | % | |
| tensile strength | Break | ISO 527-2/5 | 120 | Mpa |
| Break3 | ASTM D638 | 120 | Mpa | |
| Yield | ISO 527-2/5 | 120 | Mpa | |
| Yield3 | ASTM D638 | 120 | Mpa | |
| Tensile modulus | -- | ISO 527-2/5 | 5000 | Mpa |
| --3 | ASTM D638 | 4900 | Mpa | |
| injection | Test Condition | Test Method | Test Result | Test Unit |
| Hot air dryer | 80 | °C | ||
| Vacuum drying machine | 80 | °C | ||
| Hot air dryer | 3.0 to 4.0 | hr | ||
| Vacuum drying machine | 4.0 to 6.0 | hr | ||
| Suggested maximum moisture content | 0.040 | % | ||
| Temperature at the rear of the barrel | 260 to 270 | °C | ||
| Temperature in the middle of the barrel | 270 to 290 | °C | ||
| Temperature at the front of the material cylinder | 260 to 280 | °C | ||
| Spray nozzle temperature | 270 | °C | ||
| Mold temperature | 60 to 70 | °C | ||
| Injection pressure | 98.1 | Mpa | ||
| Back pressure | 0.981 to 1.96 | Mpa | ||
| Screw speed | 30 to 100 | rpm | ||
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Hot deformation temperature | 1.8 MPa, Unannealed, 4.00 mm | ISO 75-2/A | 97.0 | °C |
| 1.8 MPa, Unannealed, 6.40 mm | ASTM D648 | 100 | °C | |
| 0.45 MPa, Unannealed, 4.00 mm | ISO 75-2/B | 102 | °C | |
| 0.45 MPa, Unannealed, 6.40 mm | ASTM D648 | 105 | °C | |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| Shrinkage rate | Flow : 2.00 mm | ISO 294-4 | 0.10 - 0.40 | % |
| 横向Flow : 2.00 mm | ISO 294-4 | 0.10 - 0.40 | % | |
| Across FlowFlow : 3.20 mm | ASTM D955 | 0.10 - 0.40 | % | |
| Flow : 3.20 mm | ASTM D955 | 0.10 - 0.40 | % | |
| melt mass-flow rate | 300°C/1.2 kg | ASTM D1238 | 12 | g/10 min |
| 250°C/5.0 kg | ASTM D1238 | 19 | g/10 min | |
| hardness | Test Condition | Test Method | Test Result | Test Unit |
| Rockwell hardness | R -Sale | ISO 2039-2 | 120 | |
| R-Scale | ASTM D785 | 120 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.