POM CELCON® M270
32
- Properties:Low molecular weightGood forming performanceHigh mobility
- Usages:Household appliancesHousehold appliancesAutomotive sector
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|---|---|---|
DensityMelt | 内部方法 | 1.200 g/cm³ | |
SpecificHeatCapacity of Melt | 内部方法 | 2210 J/kg/°C | |
ThermalConductivityofMelt | 内部方法 | 0.16 W/m/K | |
density | ISO1183 | 1.41 g/cm³ | |
Melt volume flow rate | ISO1133 | 23.0 cm3/10min | |
Shrinkage rate | ASTMD955 | 2.2 % | |
ASTMD955 | 1.8 % | ||
ISO294-4 | 1.6 % | ||
ISO294-4 | 1.7 % | ||
Water absorption rate | ISO62 | 0.75 % | |
ISO62 | 0.20 % | ||
density | ASTMD792 | 1.41 g/cm³ |
Mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Tensile stress | ISO527-2/1A/50 | 67.0 Mpa | |
Tensile strain | ISO527-2/1A/50 | 8.0 % | |
TensileCreepModule | ISO899-1 | 2300 Mpa | |
Tensile creep modulus | ISO899-1 | 1300 Mpa | |
Flexural modulus | ISO178 | 2750 Mpa | |
Tensile modulus | ISO527-2/1A/1 | 2800 Mpa | |
tensile strength | ASTMD638 | 60.7 Mpa |
Impact resistance | Test Condition | Test Method | Test Result |
---|---|---|---|
Charpy Notched Impact Strength | ISO179/1eA | 5.2 kJ/m² | |
Impact strength of simply supported beam without notch | ISO179/1eU | 110 kJ/m² | |
ISO179/1eU | 120 kJ/m² | ||
Impact strength of cantilever beam gap | ISO180/1A | 5.4 kJ/m² |
Thermal performance | Test Condition | Test Method | Test Result |
---|---|---|---|
ASTMD648 | 110 °C | ||
ISO75-2/A | 103 °C | ||
melting temperature | ISO11357-3 | 166 °C | |
ISO11359-2 | 1.1E-04 cm/cm/°C | ||
ISO11359-2 | 1.2E-04 cm/cm/°C | ||
ISO75-2/B | 156 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.