plas
Log In

PA6 MAZMID B 150 FV20 EV10 Mazzaferro Indústria e Comércio de Polímeros e Fibras Ltda.

0
  • Properties:
    Filler glass fiber reinforced material 20% filler by weight glass beads 10% filler by weight
  • Compare

Technical Data Sheet

impact performanceTest ConditionTest MethodTest Result
Impact strength of cantilever beam gapASTM D25660to70 J/m
mechanical propertiesTest ConditionTest MethodTest Result
tensile strengthASTM D638100 MPa
elongationBreakASTM D6383.0to5.0 %
thermal performanceTest ConditionTest MethodTest Result
Continuous use temperature90.0to110 °C
Melting temperature214to220 °C
Physical propertiesTest ConditionTest MethodTest Result
densityASTM D7921.35 g/cm³
Shrinkage rateMDASTM D9550.40to0.50 %
Water absorption rate23°C,24hrASTM D5700.70to0.80 %
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.