Technical Data Sheet
Uncured Properties | Test Condition | Test Method | Test Result |
---|
Viscosity | | | 0.70 Pa·s |
GelTime | | | 30 min |
hardness | Test Condition | Test Method | Test Result |
---|
Barcol Hardness | | ASTM D2583 | 46 |
Supplementary Information | Test Condition | Test Method | Test Result |
---|
GeltoPeak | | | 11.0 min |
HAPContent | | | 45 % |
PeakExotherm | | | 220 °C |
THIXOTROPIC INDEX | | | 2.00 |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
Tensile modulus | | ISO 527-2 | 4000 MPa |
tensile strength | | ISO 527-2 | 80.0 MPa |
Tensile strain | Break | ISO 527-2 | 2.7 % |
Flexural modulus | | ISO 178 | 4000 MPa |
bending strength | | ISO 178 | 114 MPa |
Thermal performance | Test Condition | Test Method | Test Result |
---|
Heat distortion temperature | | ASTM D648 | 146 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.