physical property | Test Condition | Test Method | Test Result |
---|---|---|---|
density | ASTM D792 | 1.39 g/cm³ | |
Shrinkage rate | ASTM D955 | 0.50 % | |
ASTM D955 | 1.4 % | ||
Water absorption rate | ASTM D570 | 0.057 % |
Mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Tensile modulus | ISO 527-2 | 7280 MPa | |
tensile strength | ISO 527-2 | 101 MPa | |
Tensile strain | Break | ISO 527-2 | 1.8 % |
Flexural modulus | ISO 178 | 6360 MPa | |
bending strength | ISO 178 | 164 MPa |
Impact resistance | Test Condition | Test Method | Test Result |
---|---|---|---|
Impact strength of cantilever beam gap | ISO 180/1A | 4.2 kJ/m² |
Thermal performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Linear coefficient of thermal expansion | ASTME831 | 2.3E-05 cm/cm/°C | |
ASTME831 | 1.7E-05 cm/cm/°C | ||
ASTME831 | 1.5E-05 cm/cm/°C | ||
ASTME831 | 7.2E-05 cm/cm/°C | ||
ASTME831 | 1.1E-04 cm/cm/°C | ||
ASTME831 | 1.6E-04 cm/cm/°C | ||
ASTME831 | 1.6E-04 cm/cm/°C | ||
ASTME831 | 1.7E-04 cm/cm/°C | ||
Heat distortion temperature | ISO 75-2/B | 274 °C | |
ISO 75-2/A | 241 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.