NBR SIBUR Synthetic Rubber NBR 4055 SIBUR RUSSIA

0

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
Mooney viscosityASTM D164652to58 MU
Acrylonitrile content内部方法36.0to40.0 %
ash contentASTM D5667<0.50 %
Volatile compoundsASTM D5668<0.80 %
elastomerTest ConditionTest MethodTest Result
tensile strength YieldASTM D3189>25.0 MPa
elongationBreakASTM D3189>430 %
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.