impact performanceTest ConditionTest MethodTest ResultTest Unit
Impact strength of cantilever beam gap-18°CASTM D25659J/m
Impact strength of cantilever beam gap-34°CASTM D25643J/m
Impact strength of cantilever beam gap23°CASTM D256530J/m
mechanical propertiesTest ConditionTest MethodTest ResultTest Unit
Bending modulusASTM D790862MPa
tensile strengthYieldASTM D63819.3MPa
thermal performanceTest ConditionTest MethodTest ResultTest Unit
Hot deformation temperature0.45MPa,UnannealedASTM D64890.0°C
Physical propertiesTest ConditionTest MethodTest ResultTest Unit
melt mass-flow rate230°C/2.16kgASTM D123830g/10min
densityASTM D15050.900g/cm³
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.