PA66 A3X2G10 BK BASF MALAYSIA
48
Form:Granules | Grade:Injection grade
Properties:
High mobilityheat-resisting
Typical Applications:
Laptop caseIndustrial machinery
Product Description
Certificates(1)
Datasheet
Product Description
| Typical Applications: | Laptop case | Industrial machinery |
| Properties: | High mobility | heat-resisting |
Certificates

Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Charpy Notched Impact Strength | 23°C | ISO 179/1eA | 13 / 16 | kJ/m² |
| -30℃ | ISO 179/1eA | 11 / - | kJ/m² | |
| Impact strength of simply supported beam without notch | 23℃ | ISO 179/1eA | 55 / 55 | kJ/m² |
| -30℃ | ISO 179/1eA | 50 / - | kJ/m² | |
| Impact strength of cantilever beam gap | 23℃ | ISO 180-A | 14 / 20 | kJ/m² |
| handle | Test Condition | Test Method | Test Result | Test Unit |
| Melting temperature | ISO 11357-1/-3 | 260 | °C | |
| Melt Temperature | 290 - 300 | °C | ||
| Mold temperature | 80-90 | °C | ||
| Flammable | Test Condition | Test Method | Test Result | Test Unit |
| Glow wire combustion index (GWFI) | 厚度10mm | IEC 60695-2-12 | 960 | °C |
| Extreme Oxygen Index | ISO 4589-1/-2 | 27 | % | |
| Smoke density | EN ISO 5659-2: 2007 | 184 | ||
| smoke toxicity | NF X70-100-1/-2 | 0.36 | ||
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| Tensile modulus | ISO 527-1-2 | 16000 / 12000 | Mpa | |
| Tensile strain | ISO 527-1-2 | 180 / 130 | Mpa | |
| Tensile creep modulus | 1000hr,Strain<= 0.5%,23℃ | ISO 899-1 | * / 5400 | Mpa |
| Bending modulus | ISO 178 | 13000 / - | Mpa | |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Hot deformation temperature | 1.8 MPa | ISO 75-1/2 | 250 | °C |
| 0.45 MPa | ISO 75-1/2 | 250 | °C | |
| Linear coefficient of thermal expansion | Across Flow:23~80°C | ISO 11359-1/-2 | 40-50 | E-6/K |
| MD:23~80℃ | ISO 11359-1/-2 | 15 - 20 | E-6/K | |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| Melt Volume Flow Rate (MVR) | 275℃,5 kg | ISO 1133 | 25 | cm3/10min |
| Shrinkage rate | TD | 0.4 | % | |
| density | ISO 1183 | 1.6 | g/cm³ | |
| Viscosity value | 0.5% in 96 % H2SO4 | ISO 307 | 140 | cm³/g |
| Water absorption rate | Saturation | ISO 62 | 3.7 - 4.3 | % |
| Equilibrium,23℃,50% RH,2.00 mm | ISO 62 | 0.70 - 1.10 | % | |
| Electrical performance | Test Condition | Test Method | Test Result | Test Unit |
| Dielectric constant | 1MHz | IEC 60250 | 3.6 / 5 | |
| Dissipation factor | IEC 60093 | 1E13 / 1E10 | E-4 | |
| Volume resistivity | IEC 60093 | /1E10 | Ohm*m | |
| 表面电阻率 | IEC 60112 | 600 | ohms |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.