Ethylene Copolymer Hyflon® PFA M620 SOLVAY BELGIUM
0
- Properties:Electrical performance
- Usages:Automotive External Parts
Technical Data Sheet
Test Condition | Test Method | Test Result | |
---|---|---|---|
耗散因数 | 23°C,100kHz | ASTMD150 | <5.0E-4 |
UL阻燃等级 | UL94 | V-0 | |
极限氧指数 | ASTMD2863 | 95 % | |
耗散因数 | 23°C,50Hz | ASTMD150 | <5.0E-4 |
抗张强度 | 断裂,23°C | ASTMD1708 | >26.0 MPa |
密度 | ASTMD792 | 2.12到2.17 g/cm³ | |
熔体质量流动速率 | 372°C/5.0kg | ASTMD1238 | 2.0到5.0 g/10min |
肖氏硬度 | 邵氏D | ASTMD2240 | 55到60 |
拉伸模量 | 23°C | ASTMD1708 | 500到600 MPa |
结晶热 | DSC | 18.0到26.0 J/g | |
融合热量 | DSC | 18.0到26.0 J/g | |
表面电阻率 | ASTMD257 | >1.0E+17 ohms | |
体积电阻率 | ASTMD257 | >1.0E+17 ohms·cm | |
介电强度 | ASTMD149 | 35到40 kV/mm | |
介电常数 | 23°C,50Hz | ASTMD150 | 2.00 |
23°C,100kHz | ASTMD150 | 2.00 | |
伸长率 | 断裂,23°C | ASTMD1708 | >300 % |
弯曲寿命 | 300.0µm | ASTMD2176 | 7.0E+4到1.0E+5 Cycles |
简支梁缺口冲击强度 | ASTMD256 | 无断裂 | |
连续使用温度 | 260 °C | ||
熔融温度 | ASTMD3307 | 280到290 °C | |
结晶峰温度 | DSC | DSC | 255到265 °C |
线性热膨胀系数 | MD | ASTMD696 | 1.2E-4到2.0E-4 cm/cm/°C |
比热 | 23°C | DSC | 900到1100 J/kg/°C |
导热系数 | 40°C | ASTMC177 | 0.20 W/m/K |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.