PC GLX143-NA9C029H SABIC INNOVATIVE US
33
Form:Granules | Grade:Injection grade
Properties:
Middle flowThermal stability
Typical Applications:
Lighting applicationsPlastic bagApplication in the automotive field
Product Description
Certificates(0)
Datasheet
Product Description
| Typical Applications: | Lighting applications | Plastic bag | Application in the automotive field |
| Properties: | Middle flow | Thermal stability |
Certificates
No Data...
Technical Data Sheet
| optical performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| transmissivity | 5000μm | ASTM D1003 | 87.0 | % |
| 4000μm | ASTM D1003 | 88.0 | % | |
| 3000μm | ASTM D1003 | 89.0 | % | |
| Refractive index | ISO 489 | 1.586 | ||
| transmissivity | 6000μm | ASTM D1003 | 86.0 | % |
| turbidity | 2540μm | ASTM D1003 | <0.80 | % |
| impact performance | Test Condition | Test Method | Test Result | Test Unit |
| Suspended wall beam without notch impact strength | 23°C | ISO 180/1U | 无断裂 | |
| -30°C | ISO 180/1U | 无断裂 | ||
| Impact strength of cantilever beam gap | 23°C | ISO 180/1A | 70 | kJ/m² |
| -30°C | ISO 180/1A | 12 | kJ/m² | |
| Impact strength of simply supported beam without notch | 23°C | ISO 179/1eU | 无断裂 | |
| -30°C | ISO 179/1eU | 无断裂 | ||
| Charpy Notched Impact Strength | 23°C | ISO 179/1eA | 73 | kJ/m² |
| -30°C | ISO 179/1eA | 14 | kJ/m² | |
| flammability | Test Condition | Test Method | Test Result | Test Unit |
| Extreme Oxygen Index | ISO 4589-2 | 25 | % | |
| Burning wire flammability index | 1.00mm | IEC 60695-2-12 | 850 | °C |
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| Tensile strain | Break | ISO 527-2/50 | 120 | % |
| Yield | ISO 527-2/50 | 6.0 | % | |
| tensile strength | Break | ISO 527-2/50 | 70.0 | Mpa |
| Yield | ISO 527-2/50 | 65.0 | Mpa | |
| Tensile modulus | ISO 527-2/1 | 2350 | Mpa | |
| bending strength | ISO 178 | 90.0 | Mpa | |
| Bending modulus | ISO 178 | 2300 | Mpa | |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| 0.45MPa, unannealed, 100mm span | ISO 75-2/Be | 136 | °C | |
| 1.8MPa, unannealed, 100mm span | ISO 75-2/Ae | 125 | °C | |
| 1.8MPa, unannealed, 64.0mm span of | ISO 75-2/Af | 124 | °C | |
| Ball Pressure Test | 125°C | IEC 60695-10-2 | Pass | |
| Linear coefficient of thermal expansion | MD:23to80°C | ISO 11359-2 | 7E-05 | cm/cm/°C |
| TD:23to80°C | ISO 11359-2 | 7E-05 | cm/cm/°C | |
| thermal conductivity | ISO 8302 | 0.20 | W/m/K | |
| RTI Elec | UL 746 | 130 | °C | |
| RTI Imp | UL 746 | 125 | °C | |
| RTI | UL 746 | 125 | °C | |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| Water absorption rate | Equilibrium,23°C,50%RH | ISO 62 | 0.15 | % |
| Saturation,23°C | ISO 62 | 0.35 | % | |
| Shrinkage rate | MD1 | Internal Method | 0.50-0.70 | % |
| Melt Volume Flow Rate (MVR) | 300°C/1.2kg | ISO 1133 | 12.0 | cm3/10min |
| Electrical performance | Test Condition | Test Method | Test Result | Test Unit |
| Dielectric strength | 1.00mm11 | IEC 60243-1 | 15 | KV/mm |
| 3.20mm,in Oil | IEC 60243-1 | 17 | KV/mm | |
| Relative permittivity | 50Hz | IEC 60250 | 2.70 | |
| 60Hz | IEC 60250 | 2.70 | ||
| 1MHz | IEC 60250 | 2.70 | ||
| Dissipation factor | 50Hz | IEC 60250 | 1E-03 | |
| 60Hz | IEC 60250 | 1E-03 | ||
| 1MHz | IEC 60250 | 0.010 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.