PA66 A3HGM53 LS BK23189 BASF SHANGHAI

153

Form:Granules

Properties:
High mobilityheat-resistingFiller: Glass fiber reinf25%Filler by weight25%Filler by weight
Typical Applications:
Laptop caseIndustrial machineryMachine/mechanical componentsShell
Product Description
Certificates(0)
Datasheet

Product Description

Typical Applications:Laptop case | Industrial machinery | Machine/mechanical components | Shell
Properties:High mobility | heat-resisting | Filler: Glass fiber reinf | 25% | Filler by weight | 25% | Filler by weight

Certificates

No Data...

Technical Data Sheet

impact performanceTest ConditionTest MethodTest ResultTest Unit
Impact strength of cantilever beam gap23°CISO 1807.1kJ/m²
Impact strength of cantilever beam gap-40°CISO 1806.0kJ/m²
Charpy Notched Impact Strength23°CISO 1797.0kJ/m²
mechanical propertiesTest ConditionTest MethodTest ResultTest Unit
Bending modulus23°CISO 1787600Mpa
Tensile strainBreak,23°CISO 527-23.0%
tensile strengthBreak,23°CISO 527-2165Mpa
Tensile modulus23°CISO 527-28500Mpa
thermal performanceTest ConditionTest MethodTest ResultTest Unit
Melting temperatureISO 3146260°C
Hot deformation temperature1.8MPa,UnannealedISO 75-2/A246°C
Hot deformation temperature0.45MPa,UnannealedISO 75-2/B260°C
Physical propertiesTest ConditionTest MethodTest ResultTest Unit
Water absorption rateEquilibrium,23°C,50%RHISO 621.9%
Water absorption rateSaturation,23°CISO 626.0%
densityISO 11831.32g/cm³
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.

Sourcing & Prices

Selling & Verification

Explore Materials

Price Index

+86 0755 27873515

Room 906, Global Digital Building, No. 9 Gaoxin Middle 3rd Road, Maling Community, Yuehai Subdistrict, Nanshan District, Shenzhen, Guangdong Province, China