PPO WCD8012 BK1066 SABIC INNOVATIVE NANSHA
14
Form:Granules | Grade:Injection grade
Properties:
Non enhancedLow odor
Typical Applications:
Electronic and Electrical ApplicationsAutomotive components
Product Description
Certificates(0)
Datasheet
Product Description
| Typical Applications: | Electronic and Electrical Applications | Automotive components |
| Properties: | Non enhanced | Low odor |
Certificates
No Data...
Technical Data Sheet
| flammability | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Burning wire flammability index | 3.00mm | IEC 60695-2-12 | 850 | °C |
| Hot filament ignition temperature | 3.00mm | IEC 60695-2-13 | 825 | °C |
| Extreme Oxygen Index | ISO 4589-2 | 27 | % | |
| VW | CCP METHOD | Pass | ||
| Smoke density | Flame,0.5mmplaque,Ds,max | ASTME662 | 110 | |
| Non-Flame,0.5mmplaque,Ds,max | ASTME662 | 47 | ||
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| crack | ASTM D638 | 16.0 | Mpa | |
| Fracture, 136 ° C | CCP METHOD | 22.0 | Mpa | |
| crack | ISO 527-2/50 | 16.0 | Mpa | |
| CCP METHOD | 310 | % | ||
| ASTM D638 | 260 | % | ||
| Fracture, 136 ° C | CCP METHOD | 250 | % | |
| crack | ISO 527-2/50 | 250 | % | |
| 100mm span | 100mm | ASTM D790 | 65.0 | Mpa |
| crack | CCP METHOD | 23.0 | Mpa | |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Brittle temperature | ASTM D746 | <-40.0 | °C | |
| Hot deformation temperature | 121°C | CCP METHOD | 5.0 | % |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| melt mass-flow rate | 250°C/10.0kg | ASTM D1238 | 16 | g/10min |
| Electrical performance | Test Condition | Test Method | Test Result | Test Unit |
| Volume resistivity | ASTM D257 | 1.9E+16 | ohms·cm | |
| Dielectric strength | 2.00mm,in Oil | IEC 60243-1 | 25 | KV/mm |
| Dielectric constant | 1MHz | ASTM D150 | 2.40 | |
| Dissipation factor | 1MHz | ASTM D150 | 7E-03 | |
| Compared to the anti leakage trace index | IEC 60112 | PLC 0 | ||
| hardness | Test Condition | Test Method | Test Result | Test Unit |
| Shore hardness | ShoreA,30Sec | ASTM D2240 | 85 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.