Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|
Tightening rate | | ASTMD1895 | 1.0 |
Shrinkage rate | | ASTMD955 | 0.0到0.10 % |
Water absorption rate | | ASTMD570 | 0.17 % |
density | | ASTMD792 | 1.90到2.09 g/cm³ |
hardness | Test Condition | Test Method | Test Result |
---|
Barcol Hardness | | ASTMD2583 | 60到65 |
flammability | Test Condition | Test Method | Test Result |
---|
UL flame retardant rating | | UL94 | HB |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
tensile strength | | ASTMD638 | 31.0到37.9 MPa |
Flexural modulus | | ASTMD790 | 8960到11000 MPa |
shear strength | | ASTMD732 | 68.9到75.8 MPa |
bending strength | | ASTMD790 | 68.9到82.7 MPa |
Compression Modulus | | ASTMD695 | 379000到393000 MPa |
compressive strength | | ASTMD695 | 138到152 MPa |
Impact resistance | Test Condition | Test Method | Test Result |
---|
Impact strength of cantilever beam gap | | ASTMD256 | 270到320 J/m |
Electrical performance | Test Condition | Test Method | Test Result |
---|
arc resistance | | ASTMD495 | >180 sec |
Inclined-PlaneTracking | | ASTMD2303 | >500 min |
Thermal performance | Test Condition | Test Method | Test Result |
---|
| | ASTMD648 | >260 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.