PA66 GT3300HSL BK20 INVISTA USA
42
Form:Granules
Properties:
Thermal stabilityGood demolding performancenhanceGlass fiber reinforcedhigh strengthdimensional stability Impact modification
Product Description
Certificates(0)
Datasheet
Product Description
| Properties: | Thermal stability | Good demolding performanc | enhance | Glass fiber reinforced | high strength | dimensional stability | Impact modification |
Certificates
No Data...
Technical Data Sheet
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Melting temperature | ISO 11357-3 | 262 | °C | |
| Thermal Properties | 1.8 MPa, Unannealed | ISO 527-2/A | 247 | °C |
| Impact strength of cantilever beam gap | 23℃ | ISO 180 | 20 | kJ/m² |
| Charpy Notched Impact Strength | -40℃ | ISO 179 | 15 | kJ/m² |
| bending strength | ISO 178 | 250 | Mpa | |
| Bending modulus | ISO 178 | 7900 | Mpa | |
| Tensile strain | Break | ISO 527-2 | 4.0 | % |
| tensile strength | Break | ISO 527-2 | 170 | Mpa |
| Tensile modulus | ISO 527-2 | 10000 | Mpa | |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| Water absorption rate | 23℃, 24 hr | ISO 62 | 1.1 | % |
| Shrinkage rate | MD : 2.00 mm | % | ||
| TD : 2.00 mm | ISO 294-4 | 0.50-0.70 | % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.