Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|---|---|---|
Shrinkage rate | ASTM D955 | 2.8 % | |
ASTM D955 | 1.5 % | ||
Shore hardness | ASTM D412 | 60 | |
Shrinkage rate | ASTM D955 | 2.8 % | |
ASTM D955 | 1.5 % |
hardness | Test Condition | Test Method | Test Result |
---|---|---|---|
Shore hardness | ASTM D2240 | 60 |
Supplementary Information | Test Condition | Test Method | Test Result |
---|---|---|---|
ozone resistance | ASTM D518 | NoCracks |
elastomer | Test Condition | Test Method | Test Result |
---|---|---|---|
compression set | ASTM D395 | 18 % | |
ASTM D395 | 36 % | ||
ASTM D395 | 53 % | ||
tensile strength | ASTM D412 | 1.80 Mpa | |
ASTM D412 | 3.10 Mpa | ||
ASTM D412 | 5.00 Mpa | ||
elongation | ASTM D412 | 600 % | |
tear strength | ASTM D624 | 24.0 kN/m | |
tensile strength | ASTM D412 | 1.80 Mpa | |
ASTM D412 | 3.10 Mpa | ||
ASTM D412 | 5.00 Mpa | ||
elongation | ASTM D412 | 600 % | |
tear strength | ASTM D624 | 24.0 kN/m | |
compression set | ASTM D395 | 18 % | |
ASTM D395 | 36 % | ||
ASTM D395 | 53 % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.