EAA 3440 DUPONT USA
196
Form:Granules | Grade:Injection grade
Properties:
Heat sealing performanceHigh toughnessResistance to stress crac
Typical Applications:
Food service sectorSoft packaging composite materials Liquid packagin
Product Description
Certificates(0)
Datasheet
Product Description
| Typical Applications: | Food service sector | Soft packaging composite materials Liquid packagin |
| Properties: | Heat sealing performance | High toughness | Resistance to stress crac |
Certificates
No Data...
Technical Data Sheet
| Other performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Water vapor permeability | 38℃,90% RH | DIN 53122/2 | 0.41 | g·mm/m2/atm/24hr |
| Starting temperature of heat sealing | Internal Method | 85 | ℃ | |
| Basic Performance | Test Condition | Test Method | Test Result | Test Unit |
| melt mass-flow rate | 190℃/2.16kg | ISO 1133 | 11 | g/10min |
| 190℃/2.16kg | ASTM D-1238 | 11 | g/10min | |
| Monomer content | Internal Method | 9.7 | % | |
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| elongation | Break,Compression Molded | ASTMD638 | 600 | % |
| tensile strength | Break,Compression Molded | ASTMD638 | 17.6 | Mpa |
| Yield,Compression Molded | ASTMD638 | 7.93 | Mpa | |
| Elongation at Break | Compression Molded | ISO 527-2 | 600 | % |
| Compression Molded | ASTM D-638 | 600 | % | |
| tensile strength | Compression Molded,Break | ISO 527-2 | 17.6 | MPa |
| Compression Molded,Break | ASTM D-638 | 17.6 | MPa | |
| Yield,Compression Molded | ISO 527-2 | 7.93 | MPa | |
| Yield,Compression Molded | ASTM D-638 | 7.93 | MPa | |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Vicat softening temperature | ASTMD1525 | 81.1 | °C | |
| Melting temperature | Internal Method | 97.8 | °C | |
| Vicat softening temperature | ASTM D-1525 | 81.1 | ℃ | |
| Melting temperature | Internal Method | 97.8 | ℃ | |
| Vicat softening temperature | ISO 306 | 81.1 | ℃ | |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| Content of comonomer | Internal Method | 9.7 | % | |
| melt mass-flow rate | 190°C/2.16kg | ASTMD1238 | 11 | g/10min |
| density | ASTMD792 | 0.938 | g/cm³ | |
| ISO 1183 | 0.938 | g/cm³ | ||
| ASTM D-792 | 0.938 | g/cm³ | ||
| film | Test Condition | Test Method | Test Result | Test Unit |
| Water vapor permeability | 38°C,90%RH | DIN 53122/2 | 0.41 | g·mm/m²/atm/24hr |
| Initial sealing temperature | Internal Method | 85.0 | °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.