Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|
density | | ISO 1183 | 1.44to1.48 g/cm³ |
hardness | Test Condition | Test Method | Test Result |
---|
Shore hardness | | ISO 868 | 88to92 |
Shore hardness | | ISO 868 | 91to95 |
flammability | Test Condition | Test Method | Test Result |
---|
Limiting Oxygen Index | | ISO 4589-2 | 28to30 % |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
tensile strength | Yield | ISO 527-2 | 17.1to20.9 MPa |
Tensile strain | Break | ISO 527-2 | 230to280 % |
Electrical performance | Test Condition | Test Method | Test Result |
---|
Volume resistivity | | ASTM D257 | >5.0E+13 ohms·cm |
Volume resistivity | | ASTM D257 | 1.5E+14 ohms·cm |
Volume resistivity | | ASTM D257 | 3E+13 ohms·cm |
Thermal performance | Test Condition | Test Method | Test Result |
---|
brittle temperature | | ISO 458 | -7.00--3.00 °C |
Usage temperature | | ISO 1183 | 105 °C |
thermal stability | | ISO R182 | >200 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.