Product Description
Certificates(0)
Datasheet
Product Description
Certificates
No Data...
Technical Data Sheet
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Brittle temperature | ASTM D746 | <-60.0 | °C | |
| Vicat softening temperature | ISO 306/A | 119 | °C | |
| Melting temperature | Internal Method | 129 | °C | |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| melt mass-flow rate | 190°C/21.6kg | ISO 1133 | 15 | g/10min |
| 190°C/5.0kg | ISO 1133 | 0.60 | g/10min | |
| film | Test Condition | Test Method | Test Result | Test Unit |
| film thickness | 25 | µm | ||
| 10to50µm | ||||
| Tensile modulus | 1%Secant,MD:25μm,Blown Film | ISO 527-3 | 400 | Mpa |
| 1%Secant,TD:25μm,Blown Film | ISO 527-3 | 500 | Mpa | |
| tensile strength | MD:Break,25μm,Blown Film | ISO 527-3 | 55.0 | Mpa |
| TD:Break,25μm,Blown Film | ISO 527-3 | 50.0 | Mpa | |
| elongation | MD:Break,25μm,Blown Film | ISO 527-3 | 550 | % |
| TD:Break,25μm,Blown Film | ISO 527-3 | 750 | % | |
| Dart impact | 25μm,Blown Film | ISO 7765-1/A | 150 | g |
| Elmendorf tear strength | MD:25.0μm | ISO 6383-2 | 25.0 | kN/m |
| TD:25.0μm | ISO 6383-2 | 250.0 | kN/m |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.