PA12 1700TU96

0
  • Properties:
    Filler
    Ecomass
    USA Ecomass
  • Usages:
    Radiation shielding

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
densityASTM D79211.0 g/cm³
Shrinkage rateASTM D9550.50to0.60 %
Mechanical propertiesTest ConditionTest MethodTest Result
Tensile modulusASTM D6389650 MPa
tensile strength ASTM D63844.8 MPa
elongationBreakASTM D6381.0 %
Flexural modulusASTM D7908410 MPa
bending strengthASTM D79063.4 MPa
Impact resistanceTest ConditionTest MethodTest Result
Impact strength of cantilever beam gapASTM D25680 J/m
Thermal performanceTest ConditionTest MethodTest Result
Heat distortion temperatureASTM D648159 °C
Heat distortion temperatureASTM D648155 °C
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.