TPV Alloy Elastoprene 65A-4000 KMI Group, Inc.
0
Technical Data Sheet
| elastomer | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Permanent compression deformation | 125°C,70hr | ASTM D395 | 44 % |
| 70°C,22hr | ASTM D395 | 26 % | |
| tear strength | 23°C | ASTM D624 | 30.0 kN/m |
| elongation | Break,23°C | ASTM D412 | 490 % |
| tensile strength | Yield,23°C | ASTM D412 | 5.00 MPa |
| 100%Strain,23°C | ASTM D412 | 2.90 MPa |
| thermal performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Brittle temperature | ASTM D746 | -70.0 °C | |
| Melting temperature | 159 °C |
| Physical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| density | ASTM D792 | 0.940 g/cm³ |
| hardness | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Shore hardness | ShoreA,15Sec | ASTM D2240 | 63 |
| ShoreA,5Sec | ASTM D2240 | 65 |
| Supplementary Information | Test Condition | Test Method | Test Result |
|---|---|---|---|
| ozone resistance | ASTM D1149 | Excellent |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.