PP Homopolymer Sasol Polymers PP HMR127

0

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
densityISO 11830.905 g/cm³
melt mass-flow rateISO 11338.5 g/10min
optical performance Test ConditionTest MethodTest Result
glossASTM D2457100
Haze ratioISO 147822.5 %
Mechanical propertiesTest ConditionTest MethodTest Result
coefficient of frictionISO 82950.17
coefficient of frictionISO 82950.20
filmTest ConditionTest MethodTest Result
tensile strength ISO 527-344.0 MPa
tensile strength ISO 527-340.0 MPa
elongationISO 527-3700 %
elongationISO 527-3730 %
Dart impactISO 7765-1300 g
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.