Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|---|---|---|
density | ISO 2781 | 0.960 g/cm³ |
hardness | Test Condition | Test Method | Test Result |
---|---|---|---|
Shore hardness | Shore A | ISO 868 | 60 |
elastomer | Test Condition | Test Method | Test Result |
---|---|---|---|
compression set | ASTM D395B | 30 % | |
tensile strength | ISO 37 | 2.30 MPa | |
ISO 37 | 4.20 MPa | ||
Break | ISO 37 | 6.10 MPa | |
elongation | Break | ISO 37 | 430 % |
tear strength | ISO 34-1 | 34 kN/m | |
compression set | ASTM D395B | 26 % |
Thermal performance | Test Condition | Test Method | Test Result |
---|---|---|---|
brittle temperature | ISO 974 | -55.0 °C | |
Maximum dynamic operating temperature | 135 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.
Contact Us
Get App