Rubber Silopren® LSR 4020

0

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
densityDIN 534791.08 g/cm³
thermosettingTest ConditionTest MethodTest Result
按重量计算的混合比:1.0
按重量计算的混合比:1.0
4.0 hr
Uncured PropertiesTest ConditionTest MethodTest Result
ColorTranslucent
ColorTranslucent
DIN 53018200 Pa·s
DIN 530184300 min
DIN 53018200 Pa·s
hardnessTest ConditionTest MethodTest Result
Hardness (Shore)Shore ADIN 5350522
Supplementary InformationTest ConditionTest MethodTest Result
sulfurization10.0 min
elastomerTest ConditionTest MethodTest Result
elongationBreakDIN 535041000 %
tear strengthASTM D62415.0 kN/m
compression setDIN 5351720 %
tensile strength DIN 535046.50 MPa
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.