TPU-Ester Zythane® 5080A Alliance Polymers & Services

0

Technical Data Sheet

flammabilityTest ConditionTest MethodTest Result
UL flame retardant rating1.0mmUL 94HB
UL flame retardant rating1.5mmUL 94HB
UL flame retardant rating3.0mmUL 94HB
elastomerTest ConditionTest MethodTest Result
tensile strength100%StrainASTM D4124.00 MPa
tensile strength300%StrainASTM D412103 MPa
tensile strengthBreakASTM D41233.0 MPa
elongationBreakASTM D412680 %
Permanent compression deformation70°C,72hrASTM D395B0.32 %
tear strengthASTM D62473.6 kN/m
Permanent compression deformation24°C,22hrASTM D395B0.18 %
mechanical propertiesTest ConditionTest MethodTest Result
Taber abraserASTM D104424.0 mg
Wear resistanceDIN 5351625 mm³
thermal performanceTest ConditionTest MethodTest Result
Vicat softening temperatureASTM D152582.2 °C
Brittle temperatureDSC-37.2 °C
Physical propertiesTest ConditionTest MethodTest Result
densityASTM D7921.21 g/cm³
hardnessTest ConditionTest MethodTest Result
Shore hardnessShoreAASTM D224080
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.