Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|
density | | g/cm³ | 1.14 -- |
Water absorption rate | | % | 1.0 -- |
Water absorption rate | | % | 4.0 -- |
hardness | Test Condition | Test Method | Test Result |
---|
ball-indentation hardness | | MPa | 130 110 |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
Tensile modulus | | MPa | 2900 2300 |
tensile strength | Yield | MPa | 75.0 55.0 |
coefficient of friction | Steel - Static | | 0.14 0.20 |
tensile strength | Break | MPa | 110 50.0 |
Tensile strain | Break | % | >30 -- |
Flexural modulus | | MPa | 2700 2100 |
coefficient of friction | Steel - Dynamic | | 0.040 0.080 |
Impact resistance | Test Condition | Test Method | Test Result |
---|
Impact strength of cantilever beam gap | | kJ/m² | >6.0 >18 |
Suspended wall beam without notch impact strength | | | 无断裂 |
Electrical performance | Test Condition | Test Method | Test Result |
---|
dielectric strength | | kV/mm | 50 20 |
dielectric constant | | | 3.70 -- |
Dissipation Factor | | | 0.030 -- |
Surface Resistivity | | ohms | 1E+12 1E+10 |
Thermal performance | Test Condition | Test Method | Test Result |
---|
Heat distortion temperature | | °C | 200 -- |
Heat distortion temperature | | °C | 110 -- |
melting temperature | | °C | 200to220 -- |
Linear coefficient of thermal expansion | | cm/cm/°C | 7.0E-5到8.0E-5 -- |
specific heat | | J/kg/°C | 1670 -- |
thermal conductivity | | W/m/K | 0.25 -- |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.