LLDPE Arak LLDPE LL0209AA / LL0209KJ

0

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
densityASTMD28380.920 g/cm³
melt mass-flow rateASTMD12380.90 g/10min
optical performance Test ConditionTest MethodTest Result
glossASTMD245756
Haze ratioASTMD100310 %
filmTest ConditionTest MethodTest Result
Film thickness - tested38 µm
Available film thickness35-100µm
tensile strengthASTMD88210.5 MPa
tensile strengthASTMD88211.0 MPa
tensile strengthASTMD88241.0 MPa
tensile strengthASTMD88232.0 MPa
elongationASTMD882620 %
elongationASTMD882840 %
Falling hammer impactASTMD1709150 g
Elmondov tear strengthASTMD1922150 g
Elmondov tear strengthASTMD1922370 g
Thermal performanceTest ConditionTest MethodTest Result
vicatASTMD1525100 °C
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.