Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|
Water absorption rate | | ISO 62 | 0.85 % |
flammability | Test Condition | Test Method | Test Result |
---|
UL flame retardant rating | | UL 94 | HB |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
Tensile stress | | ISO 527-2/5 | 190 Mpa |
Tensile strain | | ISO 527-2/5 | 4.0 % |
Bending modulus 3 | | ISO 178 | 9000 Mpa |
Bending stress 3 | | ISO 178 | 290 Mpa |
injection | Test Condition | Test Method | Test Result |
---|
drying temperature | | | 80 °C |
Drying time - vacuum dryer | | | 2.0 到 6.0 hr |
Processing (melt) temperature | | | 260 到 280 °C |
Temperature | | | 80 到 120 °C |
Residual Moisture Content | | Karl Fisher | < 0.10 % |
Thermal performance | Test Condition | Test Method | Test Result |
---|
| | ISO 75-2/A | 255 °C |
Melting temperature 4 | | ISO 11357-3 | 260 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.