PA66 1402G BK ASAHI JAPAN
78
Form:Granules | Grade:Injection grade
Properties:
High rigidityhigh strengthFatigue resistanceCreep resistanceThermal stabilityModerate heat resistance
Typical Applications:
Automotive sectorElectronic fieldElectrical fieldcomponent
Product Description
Certificates(0)
Datasheet
Product Description
| Typical Applications: | Automotive sector | Electronic field | Electrical field | component |
| Properties: | High rigidity | high strength | Fatigue resistance | Creep resistance | Thermal stability | Moderate heat resistance |
Certificates
No Data...
Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Charpy Notched Impact Strength | ISO 179 | 11 | kJ/m² | |
| Impact strength of simply supported beam without notch | ISO 179 | 72 | kJ/m² | |
| Impact strength of cantilever beam gap | ASTM D256 | 130 | J/m | |
| flammability | Test Condition | Test Method | Test Result | Test Unit |
| UL flame retardant rating | 0.75 mm | UL 94 | HB | |
| Extreme Oxygen Index | ASTM D2863 | 23 | % | |
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| Tensile modulus | 23°C | ISO 527-2 | 10000 | Mpa |
| tensile strength | Break, 23°C | ISO 527-2 | 190 | Mpa |
| -- | ASTM D638 | 186 | Mpa | |
| elongation | Break | ASTM D638 | 3.0 | % |
| Break, 23°C | ISO 527-2 | 3.0 | % | |
| Bending modulus | -- | ASTM D790 | 9300 | Mpa |
| 23°C | ISO 178 | 9000 | Mpa | |
| bending strength | -- | ASTM D790 | 289 | Mpa |
| 23°C | ISO 178 | 275 | Mpa | |
| Taber abraser | 1000 Cycles | ASTM D1044 | -- | mg |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Hot deformation temperature | 0.45 MPa, Unannealed | ASTM D648 | 260 | °C |
| 0.45 MPa, Unannealed | ISO 75-2/B | 265 | °C | |
| 1.8 MPa, Unannealed | ASTM D648 | 250 | °C | |
| Linear coefficient of thermal expansion | Flow | ASTM D696 | 3.0E-5 | cm/cm/°C |
| specific heat | 1590 | J/kg/°C | ||
| thermal conductivity | 0.30 | W/m/K | ||
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| density | ASTM D792 | 1.39 | g/cm³ | |
| Shrinkage rate | 横向Flow | Internal Method | 0.90 | % |
| Flow | Internal Method | 0.40 | % | |
| Water absorption rate | Saturation, 23°C | -- | % | |
| Equilibrium, 23°C, 50% RH | ISO 62 | -- | % | |
| Electrical performance | Test Condition | Test Method | Test Result | Test Unit |
| Surface resistivity | ASTM D257 | 1.0E+15 | ohms | |
| Volume resistivity | -- | ASTM D257 | 1.0E+15 | ohms·cm |
| 23°C | IEC 60093 | 1.0E+15 | ohms·cm | |
| Dielectric strength | ASTM D149 | 28 | KV/mm | |
| hardness | Test Condition | Test Method | Test Result | Test Unit |
| Rockwell hardness | M-Scale | ASTM D785 | 96 | |
| R-Scale | ASTM D785 | 120 | ||
| M -Sale | ISO 2039-2 | 96 | ||
| R -Sale | ISO 2039-2 | 120 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.