Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|
melt mass-flow rate | | ASTMD1238 | 0.80 g/10min |
Vinyl acetate content | | | 9.5 wt% |
density | | ASTMD1505 | 0.929 g/cm³ |
optical performance | Test Condition | Test Method | Test Result |
---|
Haze ratio | | ASTMD1003 | 3.0 % |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
tensile strength | Break | ASTMD638 | 19.1 MPa |
elongation | Break | ASTMD638 | 760 % |
film | Test Condition | Test Method | Test Result |
---|
elongation | | ASTMD882 | 650 % |
Falling hammer impact | | ASTMD1709 | >400 g |
Film thickness - tested | | | 60 µm |
tensile strength | | ASTMD882 | 26.5 MPa |
tensile strength | | ASTMD882 | 24.5 MPa |
elongation | | ASTMD882 | 350 % |
TensileTearStrength | | ASTMD1004 | 78.5 kN/m |
TensileTearStrength | | ASTMD1004 | 83.4 kN/m |
Thermal performance | Test Condition | Test Method | Test Result |
---|
brittle temperature | | ASTMD746 | <-76.0 °C |
vicat | | ASTMD1525 | 77.0 °C |
| | 内部方法 | 98.0 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.