NBR NANCAR® 1203LD Nantex Industry Co., Ltd.

0

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
Mooney viscosityASTM D164666 MU
bound acrylonitrile content内部方法28.0 %
hardnessTest ConditionTest MethodTest Result
Shore hardnessShore A72
Supplementary InformationTest ConditionTest MethodTest Result
ozone resistancenocrack
elastomerTest ConditionTest MethodTest Result
tensile strength Yield12.7 MPa
elongationBreak370 %
compression set45 %
agingTest ConditionTest MethodTest Result
Change rate of tensile strength in air3.0 %
Change rate of ultimate elongation in air-38 %
Change rate of hardness (Shore) in the air2.0
Change rate of tensile strength in air14 %
Change rate of tensile strength in air12 %
Change rate of ultimate elongation in air-43 %
Change rate of ultimate elongation in air-32 %
Change rate of hardness (Shore) in the air10
Change rate of hardness (Shore) in the air2.0
volume change-12 %
volume change2.0 %
Thermal performanceTest ConditionTest MethodTest Result
Heat lossASTM D56880.30 %
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.