PA6 Staramide B28 EUROSTAR FRANCE
Product Description
Certificates(0)
Datasheet
Product Description
Certificates
No Data...
Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Charpy Notched Impact Strength | -30°C | ISO 179/1eA | 4.0 | kJ/m² |
| 23°C | ISO 179/1eA | 5.0 | kJ/m² | |
| Impact strength of simply supported beam without notch | -30°C | ISO 179/1eU | >100 | kJ/m² |
| 23°C | ISO 179/1eU | >270 | kJ/m² | |
| Impact strength of cantilever beam gap | -40°C | ISO 180/1A | 3.0 | kJ/m² |
| -20°C | ISO 180/1A | 4.0 | kJ/m² | |
| 23°C | ISO 180/1A | 5.0 | kJ/m² | |
| flammability | Test Condition | Test Method | Test Result | Test Unit |
| Extreme Oxygen Index | ISO 4589-2 | 24 | % | |
| Burning wire flammability index | 2.0mm | IEC 60695-2-12 | 960 | °C |
| UL flame retardant rating | 3.0mm | UL 94 | HB | |
| 0.75mm | UL 94 | HB | ||
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| Tensile modulus | ISO 527-2/1 | 2700 | MPa | |
| tensile strength | Yield | ISO 527-2/50 | 70.0 | MPa |
| elongation | Yield3 | ASTM D638 | 3.5 | % |
| Break | ISO 527-2/50 | >15 | % | |
| Bending modulus | ISO 178 | 2400 | MPa | |
| bending strength | ISO 178 | 85.0 | MPa | |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Hot deformation temperature | 1.8MPa,Unannealed,100mmSpan | ISO 75-2/Ae | 60.0 | °C |
| RTI Elec | UL 746 | 65.0 | °C | |
| thermal conductivity | ISO 8302 | 0.29 | W/m/K | |
| Linear coefficient of thermal expansion | TD:23to60°C | ISO 11359-2 | 8E-05 | cm/cm/°C |
| MD:23to60°C | ISO 11359-2 | 8E-05 | cm/cm/°C | |
| Ball Pressure Test | 125°C | IEC 60695-10-2 | 通过 | |
| Vicat softening temperature | -- | ISO 306/B120 | 200 | °C |
| -- | ISO 306/B50 | 210 | °C | |
| RTI | UL 746 | 65.0 | °C | |
| RTI Imp | UL 746 | 65.0 | °C | |
| Hot deformation temperature | 0.45MPa,Unannealed,100mmSpan | ISO 75-2/Be | 180 | °C |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| Water absorption rate | Equilibrium,23°C,50%RH | ISO 62 | 2.6 | % |
| Saturation,23°C | ISO 62 | 10 | % | |
| Shrinkage rate | MD | Internal Method | 1.1to1.5 | % |
| density | ISO 1183 | 1.14 | g/cm³ | |
| Electrical performance | Test Condition | Test Method | Test Result | Test Unit |
| Compared to the anti leakage trace index | SolutionB | IEC 60112 | PLC 0 | |
| -- | IEC 60112 | PLC 0 | ||
| Dissipation factor | 1MHz | IEC 60250 | 0.018 | |
| 60Hz | IEC 60250 | 5.8E-03 | ||
| Surface resistivity | IEC 60093 | >1.0E+16 | ohms | |
| Volume resistivity | IEC 60093 | >1.0E+16 | ohms·cm | |
| Dielectric strength | 3.20mm,in Oil | IEC 60243-1 | 16 | kV/mm |
| Relative permittivity | 50Hz | IEC 60250 | 3.30 | |
| 60Hz | IEC 60250 | 3.30 | ||
| 1MHz | IEC 60250 | 3.00 | ||
| Dissipation factor | 50Hz | IEC 60250 | 5.8E-03 | |
| hardness | Test Condition | Test Method | Test Result | Test Unit |
| Rockwell hardness | R-Sale | ISO 2039-2 | 120 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.