Technical Data Sheet
hardness | Test Condition | Test Method | Test Result |
---|
| | ASTMD2240 | 90 |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
| | ASTMD3389 | 40.0 mg |
elastomer | Test Condition | Test Method | Test Result |
---|
Tensile stress | | ASTMD412 | 13.8 Mpa |
tensile strength | | ASTMD412 | 34.5 Mpa |
elongation | | ASTMD412 | 550 % |
0.762mm3 | | ASTMD624 | 79.4 kN/m |
crack | | ASTMD470 | 21 kN/m |
Stretch permanent deformation | | ASTMD412 | 18 % |
Tensile stress | | ASTMD412 | 6.20 Mpa |
film | Test Condition | Test Method | Test Result |
---|
Water vapor permeability 1 | | ASTME96 | 740 g/m²/24hr |
WaterVaporTransmission-Mocon2 | | ASTMD6701 | 3000 g/m²/24hr |
Thermal performance | Test Condition | Test Method | Test Result |
---|
Glass Transition Temperature | | ASTMD3418 | -24.0 °C |
melting temperature | | DSC | 144 °C |
Kofler Melting Temperature | | 内部方法 | 135 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.