PP Homopolymer TATREN® IM 6 56

0

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
melt mass-flow rateISO 11336.5 g/10min
hardnessTest ConditionTest MethodTest Result
Rockwell hardnessR-ScaleISO 2039-288
Mechanical propertiesTest ConditionTest MethodTest Result
Tensile strainISO 527-26.0 %
Flexural modulusInjectionISO 1781500 MPa
Tensile modulusInjectionISO 527-21600 MPa
tensile strength ISO 527-227.5 MPa
Impact resistanceTest ConditionTest MethodTest Result
Impact strength of cantilever beam gapISO 180/A4.0 kJ/m²
Impact strength of cantilever beam gapISO 180/A9.0 kJ/m²
Thermal performanceTest ConditionTest MethodTest Result
Heat distortion temperatureISO 75-2/B92.0 °C
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.