POE 3200 DOW USA
89
Form:Granules | Grade:Injection grade
Properties:
High mobilityHigh impact resistance
Typical Applications:
household electrical appliancesBottle cap
Product Description
Certificates(0)
Datasheet
Product Description
| Typical Applications: | household electrical appliances | Bottle cap |
| Properties: | High mobility | High impact resistance |
Certificates
No Data...
Technical Data Sheet
| optical performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| turbidity | 2000μm,Injection | ASTM D1003 | 3.9 | % |
| gloss | 60°,1000μm,Compression Molded | ASTM D523 | 134 | |
| 20°,1000μm,Compression Molded | ASTM D523 | 125 | ||
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| Bending modulus | Compression Molded,1%Secant | ASTM D790 | 131 | Mpa |
| elongation | Break,Compression Molded | ASTM D638 | 840 | % |
| tensile strength | Break,Compression Molded | ASTM D638 | 22.1 | Mpa |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Melting temperature | Internal Method | 85.0 | °C | |
| Vicat softening temperature | ASTM D1525 | 59.0 | °C | |
| Glass transition temperature | Internal Method | -23.0 | °C | |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| Summary of Crystallinity | Internal Method | 30 | % | |
| melt mass-flow rate | 230°C/2.16kg | ASTM D1238 | 8.0 | g/10min |
| hardness | Test Condition | Test Method | Test Result | Test Unit |
| Shore hardness | ShoreD,Compression Molded | ASTM D2240 | 44 | |
| ShoreA,Compression Molded | ASTM D2240 | 94 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.