Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Impact strength of cantilever beam gap | 23°C | ISO 180/1A | 5.0 | kJ/m² |
| -20°C | ISO 180/1A | 4.0 | kJ/m² | |
| -40°C | ISO 180/1A | 3.0 | kJ/m² | |
| Impact strength of simply supported beam without notch | 23°C | ISO 179/1eU | >270 | kJ/m² |
| -30°C | ISO 179/1eU | >100 | kJ/m² | |
| Charpy Notched Impact Strength | 23°C | ISO 179/1eA | 5.0 | kJ/m² |
| -30°C | ISO 179/1eA | 4.0 | kJ/m² | |
| flammability | Test Condition | Test Method | Test Result | Test Unit |
| UL flame retardant rating | 0.75mm | UL 94 | HB | |
| Extreme Oxygen Index | ISO 4589-2 | 24 | % | |
| UL flame retardant rating | 3.0mm | UL 94 | HB | |
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| Bending modulus | ISO 178 | 2400 | MPa | |
| elongation | Break | ISO 527-2/50 | >15 | % |
| Yield2 | ASTM D638 | 3.5 | % | |
| tensile strength | Yield | ISO 527-2/50 | 70.0 | MPa |
| Tensile modulus | ISO 527-2/1 | 2700 | MPa | |
| bending strength | ISO 178 | 85.0 | MPa | |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Hot deformation temperature | 1.8MPa,Unannealed,100mmSpan | ISO 75-2/Ae | 60.0 | °C |
| 0.45MPa,Unannealed,100mmSpan | ISO 75-2/Be | 180 | °C | |
| Linear coefficient of thermal expansion | TD:23to60°C | ISO 11359-2 | 8E-05 | cm/cm/°C |
| MD:23to60°C | ISO 11359-2 | 8E-05 | cm/cm/°C | |
| Ball Pressure Test | 125°C | IEC 60695-10-2 | 通过 | |
| Vicat softening temperature | -- | ISO 306/B120 | 200 | °C |
| -- | ISO 306/B50 | 210 | °C | |
| thermal conductivity | ISO 8302 | 0.29 | W/m/K | |
| RTI Elec | UL 746 | 65.0 | °C | |
| RTI Imp | UL 746 | 65.0 | °C | |
| RTI | UL 746 | 65.0 | °C | |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| Water absorption rate | Equilibrium,23°C,50%RH | ISO 62 | 2.6 | % |
| Saturation,23°C | ISO 62 | 10 | % | |
| Shrinkage rate | MD | Internal Method | 1.1to1.5 | % |
| density | ISO 1183 | 1.14 | g/cm³ | |
| Electrical performance | Test Condition | Test Method | Test Result | Test Unit |
| Surface resistivity | IEC 60093 | >1.0E+16 | ohms | |
| Relative permittivity | 60Hz | IEC 60250 | 3.30 | |
| 1MHz | IEC 60250 | 3.00 | ||
| Volume resistivity | IEC 60093 | >1.0E+16 | ohms·cm | |
| Dielectric strength | 3.20mm,in Oil | IEC 60243-1 | 16 | kV/mm |
| Relative permittivity | 50Hz | IEC 60250 | 3.30 | |
| Dissipation factor | 50Hz | IEC 60250 | 5.8E-03 | |
| 60Hz | IEC 60250 | 5.8E-03 | ||
| 1MHz | IEC 60250 | 0.018 | ||
| Compared to the anti leakage trace index | -- | IEC 60112 | PLC 0 | |
| SolutionB | IEC 60112 | PLC 0 | ||
| hardness | Test Condition | Test Method | Test Result | Test Unit |
| Rockwell hardness | R-Sale | ISO 2039-2 | 120 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.