physical property Test ConditionTest MethodTest Result
StyreneContent42 %
Uncured PropertiesTest ConditionTest MethodTest Result
density1.13 g/cm³
0.53 Pa·s
GelTime18 min
hardnessTest ConditionTest MethodTest Result
Barcol HardnessASTMD258345
flammabilityTest ConditionTest MethodTest Result
FlameSpread-ASTME8435.0
SmokeDeveloped-ASTME84445
Supplementary InformationTest ConditionTest MethodTest Result
GeltoPeak14.0 min
PeakExotherm191 °C
ThixotropicIndex2.00
Mechanical propertiesTest ConditionTest MethodTest Result
Tensile modulusASTMD6383400 MPa
tensile strengthASTMD63858.6 MPa
elongationBreakASTMD6382.4 %
Flexural modulusASTMD7903790 MPa
bending strengthASTMD790110 MPa
Thermal performanceTest ConditionTest MethodTest Result
ASTMD648138 °C
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.