Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|
Water absorption rate | | | 0.30 % |
density | | | 1.20-1.24 g/cm³ |
STORAGE STABILITY | | | 5.0-40 min |
Thermosetting mixed viscosity | | | 1200-2000 cP |
hardness | Test Condition | Test Method | Test Result |
---|
Hardness (Shore A) | | ISO 868 | 55-60 |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
tensile strength | | ISO 527-2 | 9 MPa |
elongation at break | | ISO 527-2 | 35 % |
Flame retardant performance | Test Condition | Test Method | Test Result |
---|
Relative temperature of heating wire | | IEC 60695-2-13 | 960 °C |
UL flame retardant rating | | UL -94 | V-2 2.00mm |
UL flame retardant rating | | UL -94 | V-0 3.00mm |
GWIT | | IEC 60695-2-12 | 850 °C |
GWIT | | IEC 60695-2-12 | 850 °C |
Relative temperature of heating wire | | IEC 60695-2-13 | 960 °C |
Electrical performance | Test Condition | Test Method | Test Result |
---|
dielectric strength | | IEC 60243-1 | 28 KV/mm |
Volume resistivity | | IEC 60093 | 1E+13 Ω.cm |
dielectric constant | | IEC 60250 | 5.60 50Hz |
Thermal performance | Test Condition | Test Method | Test Result |
---|
Linear coefficient of thermal expansion | | TMA | 9 °C |
Linear coefficient of thermal expansion | | ISO 22007-2 | 0.66 W/m/K |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.