PP 3210G6 HUIZHOU NPC
201
Form:Granules | Grade:Enhanced level | Filler:glass fibre 30 %
Properties:
High rigidityGlass fiber reinforcedhigh strengthheat-resistingLow shrinkage30% glass fiber reinforceHigh rigidityLow shrinkageHigh mechanical strengthHeat resistance
Typical Applications:
Household appliancessmall home appliancesShellBobbinPump casingController housingHome appliance products etc
Product Description
Certificates(1)
Datasheet
Product Description
| Typical Applications: | Household appliances | small home appliances | Shell | Bobbin | Pump casing | Controller housing | Home appliance products | etc |
| Properties: | High rigidity | Glass fiber reinforced | high strength | heat-resisting | Low shrinkage | 30% glass fiber reinforce | High rigidity | Low shrinkage | High mechanical strength | Heat resistance |
| Filler: | glass fibre 30% |
Certificates
TDS
Technical Data Sheet
| CONDITION | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Mold temperature | - | 50 | ℃ | |
| Pressure | - | 400-800 | kg/cm2 | |
| Screw speed | - | 180 | rpm | |
| Injection speed | - | 快 | - | |
| Barrel temperature (later stage) | - | 220 | ℃ | |
| Pre drying temperature | - | 100 | ℃ | |
| Pre drying time | - | 1 | hrs | |
| Nozzle temperature | - | 230 | ℃ | |
| Barrel temperature (front section) | - | 225 | ℃ | |
| Material barrel temperature (middle section) | - | 225 | ℃ | |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Melting temperature | DSC | 165 | ℃ | |
| melt mass-flow rate | 230℃,2.16kg | ASTM D-1238 | 8.5 | g/10min |
| Hot deformation temperature | 4.6kg/cm2 | ASTM D-648 | 155 | ℃ |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| Shrinkage rate | 3mm厚度,TD | 内部标准 | 0.4~0.8 | % |
| 3mm厚度,MD | 内部标准 | 0.2~0.6 | % | |
| density | ASTM D-792 | 1.12 | - | |
| Rockwell hardness | ASTM D-785 | 88 | R | |
| Izod Notched Impact Strength | ASTM D-256 | 8.5 | kg·cm/cm | |
| Bending modulus | ASTM D-790 | 49800 | kg/cm2 | |
| bending strength | ASTM D-790 | 1200 | kg/cm2 | |
| Elongation at Break | ASTM D-638 | 3.5 | % | |
| tensile strength | Yield | ASTM D-638 | 800 | kg/cm2 |
| Electrical performance | Test Condition | Test Method | Test Result | Test Unit |
| Arc resistance | ASTM D-495 | 130 | sec | |
| Loss factor (10 ^ 6HZ) | ASTM D-150 | --- | - | |
| Dielectric constant (10 ^ 6HZ) | ASTM D-150 | 2.4 | - | |
| Dielectric strength (1mm) | ASTM D-149 | 40 | KV/mm | |
| Volume resistivity | ASTM D-257 | 10^16 | Ω·cm | |
| flame retardant performance | Test Condition | Test Method | Test Result | Test Unit |
| UL94 flame retardant rating | 0.75mm | UL 94 | HB | - |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.