Rubber Shin-Etsu Elastomer KE-7022U Shin-Etsu Silicones of America

Typical Applications:
roller
Product Description
Certificates(0)
Datasheet

Product Description

Typical Applications:roller

Certificates

No Data...

Technical Data Sheet

elastomerTest ConditionTest MethodTest ResultTest Unit
tensile strength8.41MPa
elongationBreak280%
tear strength11.4kN/m
Permanent compression deformation180°C,22hr7.0%
thermosettingTest ConditionTest MethodTest ResultTest Unit
Post curing time200°C4.0hr
Physical propertiesTest ConditionTest MethodTest ResultTest Unit
density1.29g/cm³
hardnessTest ConditionTest MethodTest ResultTest Unit
Shore hardness62
Supplementary InformationTest ConditionTest MethodTest ResultTest Unit
CureAgentDBPH
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.