PA66 A3EG10 BASF GERMANY
217
Form:Granules | Grade:Enhanced level
Properties:
Oil resistantHigh rigidity
Typical Applications:
Industrial componentsElectronic insulation
Product Description
Certificates(1)
Datasheet
Product Description
| Typical Applications: | Industrial components | Electronic insulation |
| Properties: | Oil resistant | High rigidity |
Certificates

Technical Data Sheet
| other | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| purpose | 高机械强度 | |||
| impact performance | Test Condition | Test Method | Test Result | Test Unit |
| Impact strength of simply supported beam without notch | 23℃ | kJ/m² | 11.143to19.964 | |
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| Charpy Notched Impact Strength | ISO 179/1eA | 18 | KJ/m | |
| Tensile stress | Yield | ISO 527-2 | 230 | MPa |
| bending strength | ASTM D790/ISO 178 | 360 | kg·cm/cm(J/M)ft·lb/in | |
| Bending modulus | ASTM D790/ISO 178 | 15000 | kg·cm/cm(J/M)ft·lb/in | |
| Tensile modulus | ASTM D638/ISO 527 | 16800 | kg/cm²(MPa)[Lb/in²] | |
| Impact strength of cantilever beam gap | ASTM D256/ISO 179 | 13 | kg·cm/cm(J/M)ft·lb/in | |
| tensile strength | Break,23℃ | 144.83to292.41 | MPa | |
| Tensile modulus | 23℃ | 8206.9to28000.0 | MPa | |
| Tensile strain | Break,23℃ | % | 1.9to3.1 | |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| 1.8MPa, unannealed | °C | 230to250 | ||
| transverse | mm/mm/°C | 68.6E-5-127.0E-5 | ||
| flow | mm/mm/°C | 142.2E-5-203.2E-5 | ||
| 8.0Mpa, unannealed | °C | 65to220 | ||
| Continuous use temperature | °C | 110to220 | ||
| Hot deformation temperature | 1.8Mpa | ISO 75-2 | 250 | ℃ |
| UL flame retardant rating | UL94 | HB | ||
| Hot deformation temperature | 0.45Mpa | ISO 75-2 | 250 | ℃ |
| Melting temperature | 260 | ℃(℉) | ||
| °C | 260 | |||
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| Shrinkage rate | 23℃ | % | 0.10-0.31 | |
| Balance, 23 ℃, 50% RH | % | 1.2to1.5 | ||
| Saturation, 23 ℃ | % | 3.5to5.0 | ||
| Water absorption rate | ASTM D570/ISO 62 | 3.7-4.3 | % | |
| density | ASTM D792/ISO 1183 | 1560 | ||
| Electrical performance | Test Condition | Test Method | Test Result | Test Unit |
| Volume resistivity | 23℃ | ohms·cm | 1.0E+12-1.0E+14 | |
| Dielectric strength | 23℃ | V/mil | 840 | |
| Dielectric loss | 1MHz | IEC 60250 | 0.015 | |
| Dielectric constant | 1MHz | IEC 60250 | 3.8 | |
| Volume resistivity | ASTM D257/IEC 60093 | 1E 13 | Ω.cm | |
| hardness | Test Condition | Test Method | Test Result | Test Unit |
| Ball Pressure Test | 222.76to370.34 | MPa |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.