Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|
Density | | ISO 1183 | 0.922 g/cm³ |
melt mass-flow rate | | ISO 1133 | 0.80 g/10min |
Water absorption rate | | KarlFisher | <200 ppm |
Supplementary Information | Test Condition | Test Method | Test Result |
---|
GottfertElastograph | | ISO 6502 | 0.60to0.80 N·m |
Methanol washing | | 内部方法 | <1000 ppm |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
tensile strength | | ISO 527-2/250 | >17.0 MPa |
Tensile strain | Break | ISO 527-2/250 | >450 % |
aging | Test Condition | Test Method | Test Result |
---|
Change rate of ultimate elongation in air | | IEC 60811-401 | <20 % |
Electrical performance | Test Condition | Test Method | Test Result |
---|
Volume resistivity | | IEC 60093 | >1.0E+16 ohms·cm |
dielectric strength | | IEC 60243-1 | >40 kV/mm |
dielectric constant | | IEC 60250 | 2.30 |
Dissipation Factor | | IEC 60250 | 3E-04 |
Thermal performance | Test Condition | Test Method | Test Result |
---|
thermosetting | | IEC 60811-507 | 75 % |
thermosetting | | IEC 60811-507 | 5.0 % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.