Rubber Shin-Etsu Elastomer KE-7021U Shin-Etsu Silicones of America
Typical Applications:
roller
Product Description
Certificates(0)
Datasheet
Product Description
| Typical Applications: | roller |
Certificates
No Data...
Technical Data Sheet
| elastomer | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| tensile strength | 6.00 | MPa | ||
| elongation | Break | 250 | % | |
| tear strength | 9.81 | kN/m | ||
| Permanent compression deformation | 180°C,22hr | 5.0 | % | |
| thermosetting | Test Condition | Test Method | Test Result | Test Unit |
| Post curing time | 200°C | 4.0 | hr | |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| density | 1.24 | g/cm³ | ||
| hardness | Test Condition | Test Method | Test Result | Test Unit |
| Shore hardness | 52 | |||
| Supplementary Information | Test Condition | Test Method | Test Result | Test Unit |
| CureAgent | DBPH |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.